Biphase Stainless Steel

  • SUPER DUPLEX S32760 / F55 / 1.4501

    Super Duplex S32760/ F55 , Super Duplex Alloy UNS S32760 (F55 / 1.4501) dia manana fanoherana tsara Pitting sy Crevice Corrosion ao anaty rano an-dranomasina amin'ny mari-pana ambony, omena miaraka amin'ny PREN 40<( Pitting Resistance Eqv). Ny fanoherana tsara amin'ny SCC (Stress Corrosion Cracking) amin'ny tontolo Sour sy Chloride.

  • SUPER DUPLEX 2507 kalitao avo lenta

    ● UNS S32750, F53
    ● ASTM A 240, A790, A815, A182, A 276, A 476, A789
    ● EN 1.4410
    ● Anarana iombonana hafa SAF 2507®

  • Biphase Stainless Steel

    Toerana avo lenta avo lenta singa simika Grade C Si Mn SP Cr Ni Mo Cu NW hafa tsy mihoatra ny F51 0.03 1 2 0.02 0.03 21~23 4.5~6.5 2.5~3.5 - 0.08~0.2 - - F53 0.0.0 - - F53 0.0.0 - ~ 26 6 ~8 3~5 ≤0.5 0.24~0.32 — - F55 0.03 1 1 0.01 0.03 24~26 6~8 3~4 0.5~1 0.2~0.03 0.2~0.3 0.5 ~ .035 23~28 3~6 1 ~3 - - - - A4 ...