Monel 400 Uns N04400 W.Nr.2.4360 ary 2.4361
Famoronana simika
firaka | singa | C | Si | Mn | S | Ni | Fe | Cu |
Monel 400 | Min | 63.0 | 28.0 | |||||
Max | 0.3 | 0.5 | 2.0 | 0.024 | 2.5 | 34.0 |
Toetra mekanika
Aolly Status | Faharetana amin'ny sintona Rm Mpa Min | Mamokatra hery RP 0. 2 Mpa Min | Elongation A 5% Min |
vahaolana | 745 | 325 | 40 |
Toetra ara-batana
Aolly Status | Herin'ny tensile Rm Mpa Min. | Talenta vokatra RP 0. 2 Mpa Min. | Elongation A 5% |
annealed | 480 | 170 | 35 |
Malagasy
Rod, Bar, Wire ary Forging Stock- ASTM B 164 (Rod, Bar, ary Wire), ASTM B 564 (Forgings)
Plate, Sheet ary Strip-,ASTM B 127, ASME SB 127
Pipe & Tube- ASTM B 165 (Sinao sy Tube tsy misy tombo-kase), ASTM B 725 (Tube misy sodina), ASTM B 730 (Tube misy lasantsy), ASTM B 751 (Tube misy lasantsy), ASTM B 775 (Tube misy sodina), ASTM B 829 (Tube tsy misy dikany ary Tube)
Welding Products- Filler Metal 60-AWS A5.14/ERNiCu-7;Welding Electrode 190-AWS A5.11/ENiCu-7.
Toetran'ny Monel 400
● Mahatohitra ny rano an-dranomasina sy ny etona amin’ny hafanana ambony
● Tena mahatohitra ny rano matimaty na rano an-dranomasina mikoriana haingana
● Tena mahatohitra ny fikorianan'ny harafesina amin'ny ankamaroan'ny ranomamy
● Tena mahatohitra ny asidra hydrochloric sy hydrofluoric rehefa esorina
● Manolotra fanoherana kely amin'ny asidra hydrochloric sy sulfuric amin'ny mari-pana sy fifantohana tsotra, saingy mahalana no fitaovana ho an'ireo asidra ireo
● Tena fanoherana ny sira tsy miandany sy alkaline
● Ny fanoherana ny klôro ateraky ny adin-tsaina famoretana
● Toetra mekanika tsara avy amin'ny mari-pana ambany aotra ka hatramin'ny 1020° F
● Avo fanoherana ny alkali
● Teo aloha: Alloy N-155
● Manaraka: Monel k-500 UNS N05500/ W.Nr.2.4375